| Produkt | ||||||
|---|---|---|---|---|---|---|
| Epoksylim 2K | ||||||
| 30000 mPa.s | Svart | 20 | ||||
| 13000 mPa.s Selvnivellerende | Transparent | -55 °C | 82 °C | 5 | 20 min | |
| 80000 mPa.s | Transparent | -55 °C | 82 °C | 6 | 20 min | |
| 9662 mPa.s Selvnivellerende | Transparent | -40 °C | 200 °C | 5 | 15 min | |
| 8500 mPa.s Selvnivellerende | Transparent | -55 °C | 5 | 20 min | ||
| 65000 mPa.s | Grå | -55 °C | 82 °C | 10.5 | 20 min | |
| 50000 mPa.s | Gul | -55 °C | 8 | 20 min | ||
| 55000 mPa.s | Grå | -55 °C | 82 °C | 25 | 150 min | |
| 86250 mPa.s | Grå | 90 | 10 timer | |||
| 150000 mPa.s | Grå | -253 °C | 149 °C | 90 | 8 timer | |
| 12750 mPa.s Selvnivellerende | Svart | -50 °C | 100 °C | 70 | 3 timer | |
| 10500 mPa.s Selvnivellerende | Krystallklar | -50 °C | 100 °C | 70 | 3 timer | |
| 30000 mPa.s | Hvit | 20 | ||||
| 300000 mPa.s | Hvit | -55 °C | 60 | |||
| 90000 mPa.s | Svart | 90 min | ||||
| 300000 mPa.s | Hvit | -55 °C | 200 °C | 80 | ||
| 40000 mPa.s | Gul | -40 °C | 90 °C | 100 | 7 timer | |
| Grå | -60 °C | 80 °C | 35 | |||
| 150000 mPa.s | Grå | -40 °C | 120 °C | 40 | 10 min | |
| 30000 mPa.s | Hvit | -60 °C | 80 °C | 6 | 20 min | |
| Grå | -60 °C | 100 °C | 50 | 4 timer | ||
| Smeltelim | ||||||
| 2875 mPa.s Selvnivellerende | Beige | 54 °C | 0,83 | |||
| 5000 mPa.s Selvnivellerende | Beige | 79 °C | 0,75 | |||
| 6000 mPa.s Selvnivellerende | Transparent | 60 °C | 0,67 | |||
| 7000 mPa.s Selvnivellerende | Oransje | 0,42 | ||||
| 5200 mPa.s Selvnivellerende | Brun | 104 °C | 0,83 | |||
| 10500 mPa.s Selvnivellerende | Transparent | N/A °C | N/A | |||
| Sekundlim | ||||||
| 1450 mPa.s Selvnivellerende | Transparent | -50 °C | +80 °C | 0,45 | ||
| 20 mPa.s Selvnivellerende | Transparent | -64 °C | 82 °C | 0,5 min | ||
| Metylmetakrylatlim 2K | ||||||
| 42500 mPa.s | Svart | -40 °C | 3 | 2 timer | ||
| 36000 mPa.s | Gul | -40 °C | 120 °C | 3 | 2 timer | |
| 25000 mPa.s | Blågrønn | 8 | 1 timer | |||
| 20000 mPa.s | Grønn | 10 | 20 min | |||
| 60000 mPa.s | Grønn | -40 °C | 149 °C | 5 | 20 min | |
| 20000 mPa.s | Grå | -40 °C | 200 °C | 6 | 30 min | |
| 60000 mPa.s | Grønn | -40 °C | 149 °C | 10 | 34 min | |
| 90000 mPa.s | Svart | -40 °C | 10 | 25 min | ||
| 90.000 mPa.s Selvnivellerende | Svart | -40 °C | 23 | 55 min | ||
| 40000 mPa.s | Svart | -40 °C | 200 °C | 4 | 12 min | |
| 40000 mPa.s | Svart | -40 °C | 9 | |||
| 40000 mPa.s | Svart | -40 °C | 21 | |||
| 45000 mPa.s | Blågrønn | -40 °C | 5 | 10 min | ||
| 45000 mPa.s | Grønn | -40 °C | 10 | 19 min | ||
| 40000 mPa.s | Blågrønn | -40 °C | 23 | 53 min | ||
| 83000 mPa.s | Svart | -40 °C | 200 °C | 10 | 15 min | |
| Gul | 120 °C | 5 | 15 min | |||
| Polyuretanlim 1K | ||||||
| 13000 mPa.s Selvnivellerende | Svart | 135 °C | 2 | 0,5 min | ||
| 9000 mPa.s Selvnivellerende | Hvit | 135 °C | 4 | 2,5 min | ||
| Polyuretanlim 2K | ||||||
| 22000 mPa.s | Grønn | 9 | 45 min | |||
| 25000 mPa.s | Grønn | 15 | 2 timer | |||
Limenes hardhet etter herding måles som oftest enten i Shore A eller Shore D, som begge har en skala fra 1–100.
Eksempler på Shore A og Shore D
Lim og viskositet
Når man beskriver limets egenskaper, brukes begrepet viskositet, men hva betyr det? Viskositet er et begrep som brukes til å beskrive hvor tyktflytende et lim er. Viskositeten måles som oftest ved å røre i en væske. Kraften som trengs for å røre, uttrykkes i pascal. Det er naturligvis viktig å være klar over at ulike medier endrer viskositet avhengig av om de er varme eller kalde. En væske blir for eksempel mer tyntflytende når den er varm.
Alle limene våre er målt i mPa·s (millipascal-sekund).
Nedenfor kan du se noen eksempler på kjente medier og viskositeten deres. Eksemplene begynner med vann, som har en viskositet på 1 mPa·s.
Eksempler på ulike viskositeter